A.7.3. Soft Solder, Silver-loaded (Space Quality) |
||||||
PRODUCT |
||||||
Type |
Metal Alloy; Wire, Bar and Flux-cored Wire |
|||||
Chemical Composition |
62% Sn, 2% Ag, Rem. Pb |
|||||
Manufacturer |
JL Goslar GmbH Postfach 2129, D-38611 Goslar Deutschland |
Tel: +49 (0) 5321 / 754-332 Fax: +49 (0) 5321 / 754-333 Email: h.walk@jlgoslar.de www.jlgoslar.de |
||||
EXPERIENCE & AVAILABILITY |
||||||
Development Status |
Commercial Product |
|||||
Cost Range |
Low |
|||||
Lot Reproducibility |
ECSS-Q-70-08 / 1999: 62 Tin Silver-loaded Solder, EN 29453 / 1993: S-Sn62 Pb36 Ag2 |
|||||
Space Experience |
Good |
|||||
GENERAL PROPERTIES (Physical, Mechanical, Thermal, Electrical, Optical) |
||||||
Nature |
Typical Value |
Remarks |
||||
Specific Gravity |
8.5 |
@ Room Temperature |
||||
Ultimate Tensile Strength |
63 MPa |
@ Room Temperature |
||||
Proof Stress (0.2%) |
52 MPa |
@ Room Temperature |
||||
Elongation at Break |
46% |
@ Room Temperature |
||||
Thermal Expansion Coefficient |
16.0 x 10-6 °C -1 |
@ Room Temperature |
||||
PROPERTIES RELEVANT TO SPACE USE |
||||||
Nature |
Typical Value |
Type of Test |
||||
Temperature Range |
Suitable for extensive periods at +80°C or short periods to a maximum of +120°C. |
|
||||
SPECIAL RECOMMENDATIONS |
||||||
· Not generally recommended for spacecraft use. Only used to prevent scavenging (dissolution) effect when soldering to silver-plated surface (e.g. silver plated or painted components, silver wire, etc.). |
||||||